    Öğe
    Dependency of the dendritic arm spacings and tip radius on the growth rate and composition in the directionally solidified succinonitrile-carbon tetrabromide alloys
    (ELSEVIER SCIENCE BV, 2005) Kaya, H; Cadirli, E; Keslioglu, K; Marasli, N
    Succinonitrile (SCN)-carbon tetrabromide (CTB) alloys for different concentrations of CTB (C(0)) were unidirectionally solidified with a constant temperature gradient (G = 7.5 K/mm) at different growth rates (V = 6.5-103.5 mu m/s). The primary dendrite arm spacings, secondary dendrite arm spacings and dendrite tip radius were measured as a function of growth rates and compositions. Theoretical models for the dendrite arm spacings and tip radius have been compared with the experimental observations, and a comparison of our results with the current theoretical models and previous experimental results have also been made. (c) 2005 Elsevier B.V. All rights reserved.
  • Küçük Resim Yok
    Öğe
    Solid-liquid interfacial energy in the Al-Ti system
    (ELSEVIER SCIENCE BV, 2004) Keslioglu, K; Gunduz, M; Kaya, H; Cadirli, E
    The equilibrated grain boundary groove shapes for the Al-Ti peritectic system were directly observed. From the observed grain boundary groove shapes, the Gibbs-Thomson coefficient for solid Al in Al-Ti solution has been determined to be (1.281 +/- 0.06) x 10(-7) K in with a numerical method. The solid-liquid interface energy for solid Al in Al-Ti solution has been obtained to be (170.72 +/- 16.22) x 10(-3) J m(-2) from the Gibbs-Thomson equation. The grain boundary energy for the same material has been calculated to be (332.01 +/- 35.19) x 10(-3) J m(-2) from the observed grain boundary groove shapes. (C) 2004 Elsevier B.V. All rights reserved.

| Niğde Ömer Halisdemir Üniversitesi | Kütüphane | Açık Erişim Politikası | Rehber | OAI-PMH |

Bu site Creative Commons Alıntı-Gayri Ticari-Türetilemez 4.0 Uluslararası Lisansı ile korunmaktadır.


Merkez Yerleşke Bor Yolu 51240, Niğde, TÜRKİYE
İçerikte herhangi bir hata görürseniz lütfen bize bildirin

DSpace 7.6.1, Powered by İdeal DSpace

DSpace yazılımı telif hakkı © 2002-2025 LYRASIS

  • Çerez Ayarları
  • Gizlilik Politikası
  • Son Kullanıcı Sözleşmesi
  • Geri Bildirim