Comparison of Pure and Doped TiO2 Thin Films Prepared by Sol-Gel Spin-Coating Method

Küçük Resim Yok

Tarih

2017

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

Polish Acad Sciences Inst Physics

Erişim Hakkı

info:eu-repo/semantics/openAccess

Özet

In this study, using spin-coating sol-gel method we fabricated TiO2 thin films, doped with different concentrations (1, 2, and 3 mole %) of Ce, Dy, and Eu. Characterization of the prepared samples was performed by means of the X-ray diffraction, scanning electron microscopy, ultraviolet visible absorption, and differential thermal and thermo gravimetric analysis. X-ray diffraction measurements have shown that in Eu and Dy-doped samples crystal structure consists of mixed rutile and the dominant anatase phases, however the Ce doped samples consist of anatase phase only. Scanning electron microscopy images have revealed that while average thin film thickness of the Dy-doped samples decreases with increasing concentration of Dy, the average film thicknesses of samples doped with Ce and Eu increases with increasing concentrations of these dopants. Ultraviolet visible absorption spectroscopy measurements have shown that while absorbances of the samples doped by 1 and 2 mole % of the dopants have nearly similar properties, these properties differ from each other for 3 mole % of the dopants. Finally, differential thermal and thermo gravimetric analyses have shown that the chemical reactions and weight losses of the samples have occurred at the expected temperatures.

Açıklama

3rd International Conference on Computational and Experimental Science and Engineering (ICCESEN) -- OCT 19-24, 2016 -- Antalya, TURKEY

Anahtar Kelimeler

Optical-Properties, Morphology

Kaynak

Acta Physica Polonica A

WoS Q Değeri

Q3

Scopus Q Değeri

Q4

Cilt

132

Sayı

3

Künye