dc.description.abstract | The equilibrated grain boundary groove shapes of solid Sn solution (Sn-40.14 at.% In-16.11 at.% Bi) in equilibrium with the In-Bi-Sn liquid (In-21.23 at.% Bi-19.04 at.% Sn) were observed from the quenched sample at 59 degrees C. Gibbs-Thomson coefficient, solid-liquid interfacial energy and grain boundary energy of the solid Sn solution have been determined from the observed grain boundary groove shapes. The thermal conductivity of solid phase for In-21.23 at.% Bi-19.04 at.% Sn alloy and the thermal conductivity ratio of liquid phase to solid phase at the melting temperature have also been measured with radial heat flow apparatus and Bridgman type growth apparatus, respectively. (C) 2008 Elsevier Inc. All rights reserved. | |
dc.description.sponsorship | Scientific and Technical Research Council of Turkey (TUBITAK) [105T481] | |
dc.description.sponsorship | This research was financially supported by the Scientific and Technical Research Council of Turkey (TUBITAK under Contract No: 105T481). Authors are grateful to the Scientific and Technical Research Council of Turkey (TUBITAK) for their financial supports. | |
dc.identifier.doi | 10.1016/j.matchar.2008.08.010 | |
dc.identifier.endpage | 192 | |
dc.identifier.issn | 1044-5803 | |
dc.identifier.issn | 1873-4189 | |
dc.identifier.issue | 3 | |
dc.identifier.scopus | 2-s2.0-58649103769 | |
dc.identifier.scopusquality | Q1 | |
dc.identifier.startpage | 183 | |
dc.identifier.uri | https://dx.doi.org/10.1016/j.matchar.2008.08.010 | |
dc.identifier.uri | https://hdl.handle.net/11480/5088 | |
dc.identifier.volume | 60 | |
dc.identifier.wos | WOS:000264252800004 | |
dc.identifier.wosquality | Q1 | |
dc.indekslendigikaynak | Web of Science | |
dc.indekslendigikaynak | Scopus | |
dc.institutionauthor | [0-Belirlenecek] | |
dc.language.iso | en | |
dc.publisher | ELSEVIER SCIENCE INC | |
dc.relation.ispartof | MATERIALS CHARACTERIZATION | |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | |
dc.rights | info:eu-repo/semantics/closedAccess | |
dc.subject | Crystal growth | |
dc.subject | In-Bi-Sn eutectic alloy | |
dc.subject | Surface energy | |
dc.subject | Grain boundary energy | |
dc.subject | Thermal conductivity | |
dc.title | Determination of interfacial energies of solid Sn solution in the In-Bi-Sn ternary alloy | |
dc.type | Article |